FIELD: construction.
SUBSTANCE: granulometric preparation of molybdenum ores refuse is carried out by means of grinding with subsequent classification by size with extraction of fractions of 0.063-0.042 mm and less than 0.042 mm and their mixing at the ratio of 2:3. Then the specified refuse is mixed with fusible clay and nepheline slag at the ratio of 1:(1.5-2.5):(2.5-1.5). Half-finished material is baked at the temperature of 1000-1050°C.
EFFECT: increased compression and bending strength and reduced temperature of items baking.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
CERAMIC MASS FOR FACING SLAB PRODUCTION | 2005 |
|
RU2278089C1 |
CERAMIC MIXTURE FOR MAKING FACING TILES | 2010 |
|
RU2446130C2 |
CERAMIC MASS FOR PRODUCING CLINKER BRICKS | 2021 |
|
RU2754747C1 |
CERAMIC MIXTURE FOR MAKING FACING TILE | 2013 |
|
RU2520308C1 |
CERAMIC MASS | 2022 |
|
RU2781772C1 |
METHOD OF PREPARING FACING CERAMIC TILES | 1995 |
|
RU2093491C1 |
CRUDE MIX FOR MAKING CERAMIC FACING TILE | 2009 |
|
RU2412129C1 |
CERAMIC MASS FOR PRODUCTION OF FACING TILE | 2014 |
|
RU2557031C1 |
CERAMIC MIXTURE FOR MAKING FRONT ARTICLES | 2018 |
|
RU2706285C1 |
CERAMIC COMPOSITION FOR PRODUCING FACING TILES IN ACCELERATED FIRING PROCESS | 0 |
|
SU1581710A1 |
Authors
Dates
2011-10-20—Published
2010-04-26—Filed