FIELD: process engineering.
SUBSTANCE: this invention relates to non-sticking multilayer elastomer film and to method of its production. Proposed film comprises first fragile polymer film layer that may not expand to over 110% of its initial size without breakage or cracking, and second elastomer layer. Said first layer is bonded with first surface of said second elastomer layer. First layer represents polystyrene while second layer is selected from the group comprising block-copolymer of styrene and elastomer of polyolefin. Multilayer may be activated by breaking first fragile polymer layer and imparting elastoplasticity to multilayer film. Film layer that may expand to approx. 150% of its initial size and recover after expansion to not over 120% of its initial size. Proposed method comprises producing non-sticking multilayer film layer and activating non-sticking multilayer film with destruction of fragile polymer film layer along with imparting elastoplasticity to multilayer film.
EFFECT: possibility to roll elastomer film and store without its sticking.
19 cl, 8 dwg, 2 ex
Title | Year | Author | Number |
---|---|---|---|
ELASTOMERIC LAYERED MATERIALS NOT REQUIRING MECHANICAL ACTIVATION | 2008 |
|
RU2453440C2 |
EXTRUDED MULTILAYER MATERIAL FOR ABSORBENT PRODUCTS | 2009 |
|
RU2474406C2 |
METHODS OF MANUFACTURING MULTILAYER ELASTOMERIC LAMINATES, AND LAMINATES | 2006 |
|
RU2405677C2 |
EXTRUSION GLUED LAMINATES FOR ABSORBENT PRODUCTS | 2009 |
|
RU2492840C2 |
PROCESSING SURFACES OF ELASTOMER FILMS WITH COATINGS TO PREVENT CREASING IN ROLL | 2006 |
|
RU2433147C2 |
STRETCHING MULTILAYER MATERIALS | 2016 |
|
RU2707783C2 |
METHOD OF PRODUCING MULTI-FUNCTIONAL ELASTIC LAMINAR MATERIAL | 2005 |
|
RU2368501C2 |
PULL-TAB FOR ELASTIC FASTENER | 2003 |
|
RU2316301C2 |
CONTAINING STRETCHABLE ELASTIC MATERIALS CONTAINING THREADS AND FILM | 2016 |
|
RU2707774C1 |
ENVIRONMENTALLY FRIENDLY POLYMER FILMS | 2014 |
|
RU2610599C1 |
Authors
Dates
2011-11-27—Published
2006-05-12—Filed