FIELD: chemistry.
SUBSTANCE: invention can be used in chemical industry. The method of producing jointly ground calcium carbonate material, which contains ground calcium carbonate (GCC) and precipitated calcium carbonate (PCC) with coefficient of curvature at least equal to approximately 30, preferably at least approximately 40 and even more preferably at least approximately 45, comprises the following steps: a) obtaining at least one calcium carbonate material, optionally, in form of an aqueous suspension; b) combined grinding of GCC and PCC, optionally, with at least another mineral material which is selected from talc, clay, Al2O3, TiO2 or mixtures thereof; c) optional sieving and/or concentration of the jointly ground calcium carbonate obtained after step (b); d) optional drying of the jointly ground calcium carbonate material obtained after step (b) or (c). The coefficient of curvature is defined as d30/d70×100, where d30 and d70 denote equivalent spherical diameters, relative which 30 wt % and 70 wt % particles have a smaller size.
EFFECT: invention enables to improve optical properties of enamel paper and exclude the PCC deagglomeration step.
40 cl, 2 tbl, 4 ex
Authors
Dates
2012-01-10—Published
2006-09-12—Filed