FIELD: metallurgy.
SUBSTANCE: method involves supply of charge, melting, oxygen blowing, addition of lime with content of active lime of not less than 85% and coke during melting process and oxygen blowing. Lime with content of active lime of 40-70% together with metal junk is added to the furnace to the charge. Coke with particles with size of 5-40 mm is added during melting process and blowing process. Coke with particles with size of 0-3 mm is added after melting process is finished.
EFFECT: reduction of duration of melting process and electric power consumption.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MELTING OF CARBONIC AND LOW ALLOYED GRADES OF STEEL | 2006 |
|
RU2336310C2 |
METHOD OF STEELMAKING IN ARC FURNACE | 2013 |
|
RU2542157C1 |
METHOD OF STEEL PRODUCTION | 0 |
|
SU901288A1 |
METHOD OF SMELTING STEEL | 0 |
|
SU1370150A1 |
DUPLEX PROCESS FOR STAINLESS STEEL MELTING | 2003 |
|
RU2268310C2 |
METHOD FOR STEEL MAKING IN 100-t ELECTRIC ARC FURNACES | 1992 |
|
RU2044062C1 |
PROCEDURE FOR MELTING RAIL STEEL | 2009 |
|
RU2398889C1 |
PROCEDURE FOR STEEL MELTING | 2009 |
|
RU2409682C1 |
PROCEDURE FOR RAIL STEEL MELTING | 2009 |
|
RU2400541C1 |
0 |
|
SU537116A1 |
Authors
Dates
2012-05-20—Published
2011-04-13—Filed