FIELD: metallurgy.
SUBSTANCE: cooling of working layer of rim during the first 180 sec is performed at discrete increase in flow rate of cooler of 0.0005 to 0.02 l/(cm2/s) by 0.0001 l(cm2/s) every 15-30 sec and the next 120 sec at constant flow rate of cooler to 0.5 l/(cm2/s), and cooling of end surface of rim on the ridge side is performed with air with flow rate of 0.5 m3/(cm2/s); then, wheel is cooled in the air and tempering is performed.
EFFECT: high application properties of railroad wheels owing to improving wear resistance of working layer of wheel rim and mechanical properties of wheel disc; heating to austenisation temperature and differentiated cooling of working layer of rim and its face on the ridge side is performed during 300 s.
1 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF HEAT TREATMENT OF RAILWAY WHEELS MADE OF STEEL | 2023 |
|
RU2825657C1 |
RAILROAD WHEEL HEAT TREATMENT METHOD | 2017 |
|
RU2668872C1 |
METHOD FOR HEAT TREATMENT OF RAILWAY WHEELS | 2020 |
|
RU2763906C1 |
METHOD OF THERMAL TREATMENT OF RAILWAY WHEELS | 1998 |
|
RU2140997C1 |
METHOD OF HEAT TREATMENT OF RAILWAY WHEELS MADE OF STEEL | 2023 |
|
RU2821214C1 |
HEAT TREATMENT OF RAILWAY BANDS | 2010 |
|
RU2547375C2 |
METHOD OF HEAT TREATMENT OF SOLID-ROLLED RAILROAD WHEELS FROM ALLOYED STEEL | 2016 |
|
RU2616756C1 |
METHOD OF HEAT TREATMENT OF WHOLE-ROLLED RAILWAY WHEELS | 2016 |
|
RU2632507C1 |
METHOD OF THERMAL STRENGTHENING OF RAILWAY WHEELS | 2007 |
|
RU2353672C1 |
METHOD FOR HEAT TREATMENT OF RAILWAY WHEELS | 2016 |
|
RU2636777C1 |
Authors
Dates
2012-05-20—Published
2010-03-29—Filed