FIELD: chemistry.
SUBSTANCE: solution for chemical deposition of composite coating contains the following components, g/l: nickel sulphate 10-30, sodium hypophosphite 10-20, sodium acetate 10-15, polyvinyl alcohol 0.5-1, nanofibre 0.1-10, distilled water - 1 litre. The nanofibre is added to the solution in form of powder particles of aluminium oxide-hydroxide phases with particle size 100-700 nm.
EFFECT: invention enables to obtain a composite coating, having low coefficient of friction, high wear resistance and high corrosion resistance.
1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MULTILAYER COMPOSITE COATING MANUFACTURING ON STEEL BY CHEMICAL DEPOSITION | 2013 |
|
RU2544334C1 |
SOLUTION FOR CHEMICAL DEPOSITION OF COMPOSITE COATING | 2012 |
|
RU2509176C1 |
SOLUTION TO PRODUCE COMPOSITE COATING | 2012 |
|
RU2491370C1 |
MULTI-LAYER COMPOSITE COATING ON STEEL PRODUCED BY METHOD OF CHEMICAL DEPOSITION | 2013 |
|
RU2547518C1 |
SOLUTION FOR CHEMICAL PRECIPITATION OF COMPOSITE NICKEL-PHOSPHORUS COATINGS | 2013 |
|
RU2531219C1 |
SOLUTION FOR CHEMICAL PRECIPITATION OF COMPOSITE NICKEL COVERS | 2003 |
|
RU2235803C1 |
SOLUTION USED FOR CHEMICAL DEPOSITION OF COMPOSITE NICKEL COATINGS | 2011 |
|
RU2465374C1 |
METHOD FOR PRODUCING NICKEL-DIAMOND COATING | 2016 |
|
RU2639411C2 |
COMPOSITE COATING BASED ON NICKEL WITH ULTRA-DISPERSED DIAMONDS | 2016 |
|
RU2638480C2 |
PROCEDURE FOR FABRICATION OF COMPOSITE ANTIFRICTION COATING | 2013 |
|
RU2556155C2 |
Authors
Dates
2012-05-20—Published
2011-05-16—Filed