FIELD: chemistry.
SUBSTANCE: solution for chemical deposition of a composite coating contains components in the following ratio, g/l: nickel chloride 15-25, sodium hypophosphite 15-25, sodium acetate 8-15, nanodiamond powder with particle size of 0.004-0.450 mcm 1-20, silver nitrate 0.5-2, 5% aqueous polyvinyl alcohol solution 0.5-2, fluoroplastic suspension F-4D 2-30 and distilled water - up to 1 l.
EFFECT: improved tribological properties and microhardness of the coating.
1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF RECEIVING OF NICKEL-ADAMANTINE CHEMICAL COATINGS | 2007 |
|
RU2357002C1 |
METHOD FOR PRODUCING NICKEL-DIAMOND COATING | 2016 |
|
RU2639411C2 |
COMPOSITE COATING BASED ON NICKEL WITH ULTRA-DISPERSED DIAMONDS | 2016 |
|
RU2638480C2 |
METHOD OF PRODUCTION OF METAL-DIAMOND CHEMICAL COATING | 2007 |
|
RU2375494C2 |
SOLUTION TO PRODUCE COMPOSITE COATING | 2012 |
|
RU2491370C1 |
METHOD OF MULTILAYER COMPOSITE COATING MANUFACTURING ON STEEL BY CHEMICAL DEPOSITION | 2013 |
|
RU2544334C1 |
SOLUTION FOR CHEMICAL DEPOSITION OF COMPOSITE COATING | 2011 |
|
RU2451113C1 |
COMPOSITE METAL-DIAMOND COATING, METHOD OF ITS PRODUCTION, DISPERSE SYSTEM FOR DEPOSITION OF COMPOSITE METAL-DIAMOND COATING AND METHOD FOR ITS PRODUCTION | 2019 |
|
RU2706931C1 |
COMPOSITE METAL-DIAMOND COATING, METHOD OF ITS PRODUCTION, DIAMOND-CONTAINING ADDITIVE OF ELECTROLYTE AND METHOD OF ITS PRODUCTION | 2018 |
|
RU2699699C1 |
SOLUTION USED FOR CHEMICAL DEPOSITION OF COMPOSITE NICKEL COATINGS | 2011 |
|
RU2465374C1 |
Authors
Dates
2014-03-10—Published
2012-12-21—Filed