FIELD: construction.
SUBSTANCE: in the method to prepare a light concrete mixture on a porous filler, including mixing of portland cement with an additive, a porous filler and tempering water, first a superplasticiser additive in the amount of 0.4-0.5% of portland cement mass is added into 50-60% of the total amount of tempering water and mixed with portland cement during 50-60 s, then the whole porous filler is added, such as highly light porous filler with medium density of not more than 250 kg/m3, and again mixed for 70-80 s, afterwards the remaining part of tempering water is added, and the mixture is finally mixed for 30-40 s.
EFFECT: higher uniformity of cement dough distribution along highly light filler surface and its tighter packing in concrete, increased strength of concrete and reduction of its heat conductivity.
1 ex, 1 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD OF MANUFACTURING HEAT-INSULATION PRODUCTS | 2003 | 
 | RU2254310C1 | 
| MIX FOR MANUFACTURING HEAT-INSULATING PRODUCTS | 1999 | 
 | RU2169132C1 | 
| METHOD TO PREPARE LIGHTER MASONRY MORTAR AND COMPOSITION FOR LIGHTER MASONRY MORTAR | 2012 | 
 | RU2528323C2 | 
| METHOD OF PREPARING CEMENT CONCRETE WITH DRY VEGETABLE ADDITIVE | 2024 | 
 | RU2833999C1 | 
| RAW MIXTURE FOR MANUFACTURING BUILDING MATERIAL AND ARTICLE | 2006 | 
 | RU2312839C1 | 
| CONCRETE MIXTURE | 2013 | 
 | RU2536535C1 | 
| METHOD OF MAKING EXTRA HEAVY RADIATION-PROTECTIVE HIGH-STRENGTH CONCRETE | 2010 | 
 | RU2436750C1 | 
| METHOD OF PRODUCING LIGHT CONCRETE MIX | 0 | 
 | SU1636407A1 | 
| RAW MATERIAL MIXTURE FOR PRODUCTION OF PIECE PRODUCTS FROM SAWDUST CONCRETE WITH ADDITION OF FLY ASH | 2012 | 
 | RU2570727C2 | 
| COMPLEX NANOMODIFIER FOR NON-AUTOCLAVE HARDENING AERATED CONCRETE AND AERATED CONCRETE MIXTURE CONTAINING SAID ADDITIVE | 2024 | 
 | RU2831586C1 | 
Authors
Dates
2012-06-10—Published
2010-12-17—Filed