FIELD: metallurgy.
SUBSTANCE: electrolyte for deposition of coatings by nickel-bismuth alloy contains, g/l: nickelous chloride 40-60, nickelous bismuth 5-15, trilon B 50-60, boric acid 20-30, leveller A 2-4, distilled water to get the working volume.
EFFECT: increase of electrolyte dissipating ability and increase of coating corrosion resistance.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
ELECTROLYTE FOR PRECIPITATION OF COBALT-BISMUTH ALLOY | 2001 |
|
RU2197567C1 |
BISMUTH-TIN ALLY PRECIPITATION ELECTROLYTE | 1999 |
|
RU2164967C1 |
ELECTROLYTE FOR DEPOSITION OF BISMUTH-MANGANESE ALLOY | 1997 |
|
RU2116389C1 |
ELECTROLYTE FOR DEPOSITING COPPER-NICKEL ALLOY | 1996 |
|
RU2106436C1 |
ELECTROLYTE FOR DEPOSITION OF BISMUTH-GALLIUM ALLOY | 2009 |
|
RU2410474C2 |
ELECTROLYTE FOR APPLYING BISMUTH COVERS | 1994 |
|
RU2064535C1 |
ELECTROLYTE FOR DEPOSITION OF BISMUTH-THALLIUM ALLOY | 2005 |
|
RU2291917C1 |
ELECTROLYTE FOR DEPOSITING ARGENTUM-BISMUTH ALLOY | 2002 |
|
RU2215067C1 |
ELECTROLYTE FOR ALLOY ZINC-COBALT PRECIPITATION | 1992 |
|
RU2029798C1 |
ELECTROLYTE FOR DEPOSITING SILVER-LEAD ALLOY | 2006 |
|
RU2303662C1 |
Authors
Dates
2012-07-27—Published
2011-04-06—Filed