FIELD: chemistry.
SUBSTANCE: invention relates to the industry of ceramic materials, mainly to compositions of mixtures for making bricks. The ceramic mixture of making ceramic bricks contains low-melting clay and silver-gold alloy wastes in form of cupola slag from production of mineral wool containing oxides, wt %: SiO2 - 45.7; Al2O3 - 8.9; Fe2O3 - 9.84; CaO - 21.8; MgO - 6.8; R2O - 5.78, with the following ratio of components in wt %: low-melting clay 70-90; silver-gold alloy wastes in form of cupola slag from production of mineral wool 10-30.
EFFECT: high frost resistance.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
CERAMIC MIXTURE FOR MAKING CERAMIC BRICKS | 2011 |
|
RU2466111C1 |
CERAMIC MIXTURE FOR MAKING CERAMIC BRICKS | 2006 |
|
RU2326850C2 |
CERAMIC MIXTURE FOR MAKING CERAMIC BRICK | 2012 |
|
RU2513739C1 |
CERAMIC MIXTURE FOR MAKING CERAMIC BRICKS | 2010 |
|
RU2440949C1 |
SEMIDRY PRESSING CERAMIC MIXTURE FOR MAKING BRICKS | 2010 |
|
RU2440950C1 |
CERAMIC MIXTURE FOR MAKING CERAMIC BRICKS | 2008 |
|
RU2388723C1 |
CERAMIC MIXTURE FOR MAKING CERAMIC BRICKS | 2008 |
|
RU2389706C1 |
CERAMIC MIXTURE FOR MAKING CERAMIC BRICKS | 2009 |
|
RU2398751C1 |
CERAMIC MIXTURE FOR MAKING CERAMIC BRICKS | 2008 |
|
RU2389707C1 |
CERAMIC MIXTURE FOR MAKING CERAMIC BRICKS | 2009 |
|
RU2417196C1 |
Authors
Dates
2012-11-10—Published
2011-04-14—Filed