FIELD: metallurgy.
SUBSTANCE: method for extracting copper from sulphide-bearing ore involves ore crushing, leaching of copper with water sulphuric acid solution at pH equal to 1.5-2.0 and temperature of 25-30°C in presence of thionic bacteria with air aeration. At that, crushing is performed up to ore fractions size of 10-25 mm. Prior to leaching, sulphide-bearing ore is treated with silicate bacteria at temperature of 25-30°C and pH=6-7.
EFFECT: improving copper extraction degree at leaching.
3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR UNDERGROUND LIXIVIATION OF SULFIDE COPPER-BEARING POLYMETAL ORES | 1997 |
|
RU2124632C1 |
HEAP BIOLOGICAL LEACHING LEAN REFRACTORY MINERAL RAW MATERIALS OF NATURAL AND TECHNOGENIC ORIGIN | 2017 |
|
RU2679724C1 |
METHOD OF HEAP BACTERIAL LEACHING OF SULPHIDE CONTAINING PRODUCTS | 2007 |
|
RU2336341C1 |
METHOD OF MANGANESE HEAP BIOLEACHING OF MANGANESE-CONTAINING MATERIALS | 2018 |
|
RU2686158C1 |
METHOD FOR INTEGRATED PROCESSING OF PERSISTENT GOLD-CONTAINING MATERIAL | 2003 |
|
RU2226560C1 |
METHOD FOR PROCESSING OF SULPHIDE ORES AND PYRRHOTINE CONCENTRATE | 2008 |
|
RU2367691C1 |
METHOD OF LEACHING OF SULPHIDE CONTAINING PRODUCTS | 2007 |
|
RU2336340C1 |
METHOD OF THE URANIUM LEACHING FROM THE ROCKS WITH ITS INSIGNIFICANT CONTENT | 2016 |
|
RU2653400C2 |
METHOD OF VAT BACTERIAL LEACHING OF SULPHIDE CONTAINING PRODUCTS | 2007 |
|
RU2337156C1 |
METHOD FOR HEAP BACTERIAL LEACHING OF SULPHIDE-BEARING ORE | 2007 |
|
RU2339709C1 |
Authors
Dates
2012-12-27—Published
2011-06-10—Filed