FIELD: metallurgy.
SUBSTANCE: proposed process comprises crushing and grinding the ore, sulfuric acid leaching with addition of nitrogen acid as an oxidiser. Then, uranium is extracted and cleaned of impurities with the help of extractive agents mix to wash saturated extractive agent with the solution of sulfuric acid. After extraction, uranium is re-extracted to obtain uranium concentrate by means of 8-10%-solution of sodium carbonate. Uranium is deposited from re-extracted product by hydrogen peroxide with 50-100%-surplus from stoichiometry at equilibrium pH 3.6-4.2, mixing interval of 1- 1.5 h and sedimentation time of, at least, 1 h.
EFFECT: high quality finished uranium protoxide-oxide product.
4 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
PROCEDURE FOR PROCESSING URANIUM ORE | 2010 |
|
RU2434961C1 |
URANIUM ORE PROCESSING METHOD | 2002 |
|
RU2239668C2 |
TREATMENT METHOD OF CONCENTRATES OF NATURAL URANIUM | 2007 |
|
RU2360988C2 |
URANIUM EXTRACTION AFFINAGE PROCESS | 2005 |
|
RU2295168C1 |
METHOD OF EXTRACTION URANIUM REFINING | 2013 |
|
RU2554830C2 |
METHOD OF EXTRACTING BERYLLIUM BY ION EXCHANGE | 2014 |
|
RU2571763C1 |
METHOD OF EXTRACTION OF URANIUM FROM ORE | 2000 |
|
RU2205885C2 |
METHOD OF EXTRACTION PROCESSING OF URANIUM-CONTAINING SOLUTIONS | 1997 |
|
RU2114469C1 |
EXTRACTION METHOD FOR PROCESSING URANIUM-CONTAINING SOLUTIONS | 2022 |
|
RU2793956C1 |
METHOD OF THE NATURAL URANIUM CHEMICAL CONCENTRATE PROCESSING | 2003 |
|
RU2315716C2 |
Authors
Dates
2013-05-10—Published
2012-02-06—Filed