FIELD: metallurgy.
SUBSTANCE: proposed method comprises using filler rods made from titanium welding wire BT6"cв", micro arc oxidising in aqueous electrolyte first with NaAlO2 solution in concentration of 14÷16 g/l, pH 11.5÷12 at 280÷300 V and 20÷24°C for (15±1) minutes and, then, in aqueous electrolyte with Na3PO4 in concentration of 13÷15 g/l, pH 10.5÷11 at 290÷310 V and 16÷20°C for (18±1) minutes.
EFFECT: higher hardness of deposited metal.
1 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MICRO ARC OXIDATION OF RODS FROM TITANIUM WIRE FOR IMPLEMENTATION OF WEAR-RESISTANT PADS | 2016 |
|
RU2625516C1 |
METHOD OF MICROARC OXIDATION OF TITANIUM WIRE FOR ANTIFRICTION WELDUP | 2008 |
|
RU2391449C1 |
OXIDATION METHOD OF TITANIUM ALLOY FOR ANTIFRICTIONAL BUILDING-UP | 2008 |
|
RU2367728C1 |
METHOD OF BUILDING UP ANTIFRICTION LAYERS | 2009 |
|
RU2427455C2 |
METHOD OF RECONDITIONING WORN-OUT ALUMINIUM AND ALUMINIUM ALLOY PARTS | 1996 |
|
RU2119420C1 |
METHOD FOR RESTORATION OF WORN RESTING PLANES OF ALUMINUM ALLOY HEADS OF BLOCK OF INTERNAL COMBUSTION ENGINES | 2004 |
|
RU2274537C1 |
METHOD OF ARC DEPOSITION OF COPPER AND COPPER ALLOYS ON STEEL | 2011 |
|
RU2470750C1 |
METHOD OF ARGON-ARC WELDING OF COPPER AND ITS ALLOYS ON STEEL BY NONCONSUMABLE ELECTRODE | 2008 |
|
RU2390398C1 |
WELDING WIRE COMPOSITION | 2007 |
|
RU2346797C1 |
BUILDING UP OF WEAR RESISTANT COATS | 2009 |
|
RU2416501C2 |
Authors
Dates
2013-05-27—Published
2011-10-03—Filed