FIELD: metallurgy.
SUBSTANCE: method of micro arc oxidation (MAO) of bars made from titanium wire of "ВТ6св" grade for the products wear-resistant pads from titanium alloys, that work for a long time under the hard modes of cyclic loading, includes the electrolytic process, proceeding at the voltage of 290÷310 V, while MAO is carried out in the aqueous electrolyte with the solution of Na3PO4 and concentration of 14 g/l, pH 10.5÷11 at the temperature of 20°C for (150±10) minutes.
EFFECT: development of the titanium alloy micro arc oxidation method for the wear-resistant pads, which allows to increase the weld deposit hardness.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MICRO ARC OXIDISING OF TITANIUM ALLOY BARS FOR ANTIFRICTION WELD DEPOSITION | 2011 |
|
RU2483146C1 |
METHOD OF MICROARC OXIDATION OF TITANIUM WIRE FOR ANTIFRICTION WELDUP | 2008 |
|
RU2391449C1 |
OXIDATION METHOD OF TITANIUM ALLOY FOR ANTIFRICTIONAL BUILDING-UP | 2008 |
|
RU2367728C1 |
METHOD OF BUILDING UP ANTIFRICTION LAYERS | 2009 |
|
RU2427455C2 |
PROCEDURE FOR STRENGTHENING SEATS OF VALVES OF INTERNAL COMBUSTION ENGINES OUT OF ALUMINIUM ALLOY | 2008 |
|
RU2390587C2 |
PRODUCTION OF COATINGS ON SURFACES OF METALS AND ALLOYS | 2013 |
|
RU2547372C2 |
METHOD FOR RESTORING WORN PARTS OF ALUMINUM ALLOYS | 2004 |
|
RU2252122C1 |
METHOD OF RECONDITIONING WORNOUT PARTS FROM ALUMINIUM ALLOYS | 2009 |
|
RU2389593C1 |
PROCEDURE FOR APPLICATION OF COATING ON HARDMETAL | 2015 |
|
RU2615941C1 |
METHOD FOR RESTORATION OF WORN RESTING PLANES OF ALUMINUM ALLOY HEADS OF BLOCK OF INTERNAL COMBUSTION ENGINES | 2004 |
|
RU2274537C1 |
Authors
Dates
2017-07-14—Published
2016-03-01—Filed