FIELD: metallurgy.
SUBSTANCE: method includes heating of kyanite to 1250-1350°C. At the same time kyanite prior to heating is mixed with solid carbon at the weight ratio from 1:0.37 to 1:1.85. Heating is carried out in atmosphere of halogen-containing gases. Produced halogenides are cooled and separated, afterwards a mixture is prepared from them with required content in the product of aluminium, silicon and other chemical elements available in kyanite. Then the mixture of halogenides is heated either in atmosphere of oxygen with production of complex oxides or in recovery atmosphere with production of alloys.
EFFECT: complex wasteless processing of kyanite concentrate.
5 cl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
PRODUCTION OF SILICON WITH THE USE OF ALUMINIUM SUBCHLORIDE | 2012 |
|
RU2519460C1 |
METHOD OF PRODUCING TITANIUM CARBIDE | 2012 |
|
RU2495826C1 |
METHOD OF OBTAINING ALUMINIUM DODECABORIDE | 2012 |
|
RU2513402C2 |
METHOD OF ALUMINUM-SILICON ALLOY PRODUCTION | 1999 |
|
RU2148670C1 |
METHOD OF KYANITE CONCENTRATE RECYCLING | 2013 |
|
RU2518807C1 |
METHOD OF PRODUCTION OF ALUMINUM-SILICON ALLOY AND OTHER METALS FROM CHARGE CONTAINING ALUMINUM OXIDE | 2001 |
|
RU2203970C2 |
METHOD OF PROCESSING KYANITE CONCENTRATE | 2012 |
|
RU2489503C1 |
METHOD OF PRODUCING CORDIERITE MIXTURE FOR TECHNICAL CERAMICS | 2013 |
|
RU2521873C1 |
0 |
|
SU353781A1 | |
METHOD OF PREPARING ANTIOXIDANT | 1998 |
|
RU2147565C1 |
Authors
Dates
2013-07-10—Published
2012-01-10—Filed