FIELD: metallurgy.
SUBSTANCE: electrolyte contains the following, g/l: nickel chloride 200-350, cobalt chloride 2-10, boric acid 25-40, chloramine B 1.5-3.0, silicon oxide 1-30, fluoroplastic emulsion F-4D 7-35.
EFFECT: obtaining microcrystalline, uniform, self-lubricating coatings with high wear resistance and microhardness.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
GALVANIC NICKEL-BASED COMPOSITE MATERIAL | 2012 |
|
RU2489531C1 |
COMPOSITION NICKEL COBALT FTOROPLASTIC COATING ELECTROLYTE | 2008 |
|
RU2352694C1 |
GALVANIC NICKEL COMPOSITE | 2008 |
|
RU2352693C1 |
ELECTROLYTE FOR DEPOSITION OF COMPOSITION NICKEL-FLUOROPLASTIC COATING | 2005 |
|
RU2297476C1 |
PROCEDURE FOR PRODUCTION OF COMPOSITE ELECTRO-PLATE NICKEL-COBALT-ALUMINIUM OXIDE AND COMPOSITE ELECTRO-PLATE NICKEL-COBALT- ALUMINIUM OXIDE | 2009 |
|
RU2418107C2 |
ELECTROLYTE FOR DEPOSITION OF NICKEL-BORON-FLUOROPLASTIC COMPOSITE MATERIAL | 2002 |
|
RU2213812C1 |
METHOD OF OBTAINING COMPOSITE ELECTROCHEMICAL COATING ON STEEL | 2015 |
|
RU2618679C1 |
ELECTROPLATING NICKEL-BASE COMPOSITE MATERIAL | 2002 |
|
RU2213813C1 |
ELECTROLYTE FOR DEPOSITION OF COMPOSITE COATS BASED ON NICKEL | 1995 |
|
RU2089678C1 |
ELECTROLYTE FOR SEDIMENTATION OF COMPOSITION COATING NICKEL-COBALT-DIAMOND | 2008 |
|
RU2362843C1 |
Authors
Dates
2013-08-10—Published
2012-04-26—Filed