FIELD: chemistry.
SUBSTANCE: electrolyte contains g/l: nickel chloride 200-350, cobalt chloride 2-10, boric acid 25-40, fluoroplastic emulsion F-4D-E 7-35, chloramine 1.5-4.5 and water.
EFFECT: improved wear resistance.
2 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
GALVANIC NICKEL COMPOSITE | 2008 |
|
RU2352693C1 |
ELECTROLYTE FOR DEPOSITION OF NICKEL-COBALT-SILICON OXIDE-PLASTIC FLUOR COMPOSITE COATING | 2012 |
|
RU2489530C1 |
ELECTROLYTE FOR DEPOSITION OF COMPOSITION NICKEL-FLUOROPLASTIC COATING | 2005 |
|
RU2297476C1 |
GALVANIC NICKEL-BASED COMPOSITE MATERIAL | 2012 |
|
RU2489531C1 |
ELECTROLYTE FOR DEPOSITION OF NICKEL-BORON-FLUOROPLASTIC COMPOSITE MATERIAL | 2002 |
|
RU2213812C1 |
ELECTROPLATING NICKEL-BASE COMPOSITE MATERIAL | 2002 |
|
RU2213813C1 |
PROCEDURE FOR PRODUCTION OF COMPOSITE ELECTRO-PLATE NICKEL-COBALT-ALUMINIUM OXIDE AND COMPOSITE ELECTRO-PLATE NICKEL-COBALT- ALUMINIUM OXIDE | 2009 |
|
RU2418107C2 |
ELECTROLYTE FOR SEDIMENTATION OF COMPOSITION COATING NICKEL-COBALT-DIAMOND | 2008 |
|
RU2362843C1 |
ELECTROLYTE TO DEPOSIT COMPOSITE COATING OF ZINC AND FLUOROPLASTIC | 2011 |
|
RU2464363C1 |
ELECTROLYTE FOR SEDIMENTATION OF COMPOSITE COATING NICKEL-BORON-ALUMINIUM OXIDE | 2009 |
|
RU2418106C2 |
Authors
Dates
2009-04-20—Published
2008-03-19—Filed