FIELD: metallurgy.
SUBSTANCE: iron-containing product of a benefication process is treated with 70-80% of a bischofite solution in the form of aerosol. Surface of particles of iron-containing product is wetted with bischofite solution at its consumption in the quantity of 8-17 kilograms per ton of wet loose material.
EFFECT: high effectiveness of congelation prevention of iron-containing product under low temperature conditions.
3 cl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
IRON ORE BENEFICATION METHOD | 2011 |
|
RU2500822C2 |
METHOD FOR ANTI-FREEZING OF WET IRON ORE CONCENTRATE | 2019 |
|
RU2743951C1 |
PROCEDURE FOR DRYING FINE GRAIN IRON ORE CONCENTRATE | 2009 |
|
RU2425155C2 |
METHOD FOR OBTAINING IRON FROM OOLITES OF LIMONITE ORE AND DEVICE FOR ITS IMPLEMENTATION | 2020 |
|
RU2743132C2 |
METHOD OF INCREASING IRON-ORE CONCENTRATE PRODUCTION EFFICIENCY | 2010 |
|
RU2443474C1 |
POWDERED MAGNETIC SORBENT FOR OIL GATHERING | 2018 |
|
RU2710334C2 |
METHOD FOR IRON-ORE CONCENTRATE PROCESSING AND IRON-ORE CONCENTRATE MANUFACTURING LINE | 2009 |
|
RU2451757C2 |
IRON-ORE RAW MATERIAL BENEFICATION METHOD | 2013 |
|
RU2540173C2 |
METHOD FOR LUMPING SMALL-DISPERSED IRON-CONTAINING MATERIAL FOR METALLURGIC CONVERSION BY USING ORGANIC BINDING AGENT | 2005 |
|
RU2272848C1 |
METHOD FOR PRODUCING GRANULAR IRON CONCENTRATE | 2023 |
|
RU2806142C1 |
Authors
Dates
2013-12-10—Published
2011-02-28—Filed