FIELD: chemistry.
SUBSTANCE: porcelain mixture contains, wt %: clay 6.0-10.0; kaolin 13.0-19.0; pegmatite 31.0-33.0; quartz 23.0-25.0; potsherd 3.0-5.0; zircon 11.0-13.0; mullite 3.0-5.0. The articles have softening coefficient of 0.93-0.97.
EFFECT: high water-resistance of articles made from the porcelain mixture.
1 tbl