FIELD: construction.
SUBSTANCE: in the method to prepare an asphalt-concrete mix by means of mixing of heated mineral components, bitumen and an additive with usage of oil sludge, the additive is a finely dispersed powder, produced intense mixing of a working agent with oil sludge at their ratio of 1.5:1 with addition of water for full lime slaking, treatment of produced product with carbonic acid gas for 10-15 minutes and soaking under tight conditions for 18-30 hr, where the working agent is produced by mixing, wt %: animal fat 1-3, adsorbent produced by pyrolysis of worn car tyres at 850-1100°C with subsequent separation of metal cord and grinding to 10-3÷10-5 m, 18-22, burnt lime ground to 10-3÷10-5 m, balance, with content of bitumen of 66-83% of the mass of the specified additive, mineral components are heated to 70-90°C, the mixture of bitumen with the specified additive - up to 90-100°C, and mixing of all these mixture components is carried out during heating of up to 140-170°C.
EFFECT: improved parameters of an asphalt-concrete mixture by water resistance and water saturation.
1 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
OILY WASTE RECYCLING METHOD | 2008 |
|
RU2354670C1 |
ROAD CONCRETE MIX MAKING METHOD | 2012 |
|
RU2520256C1 |
METHOD OF SOIL RECOVERY CONTAMINATED WITH OIL | 2018 |
|
RU2694491C1 |
METHOD FOR OIL-CONTAINING SOIL RECOVERY BY CHEMICAL TREATMENT | 2018 |
|
RU2695151C2 |
METHOD FOR OIL-CONTAINING SOIL RECOVERY BY CHEMICAL TREATMENT | 2018 |
|
RU2690425C1 |
METHOD FOR OIL-CONTAINING SOIL RECOVERY BY CHEMICAL TREATMENT | 2017 |
|
RU2706945C2 |
METHOD FOR OIL-CONTAINING SOIL RECOVERY BY CHEMICAL TREATMENT | 2018 |
|
RU2705901C2 |
METHOD OF OBTAINING OF HYDROPHOBIC ADDITIVE FOR BITUMEN CONCRETE MIX AND THE METHOD OF OBTAINING BITUMEN CONCRETE MIX WITH ITS USE | 2014 |
|
RU2550767C1 |
MODIFIER COMPOSITION FOR ASPHALT MIXTURES | 2016 |
|
RU2656484C1 |
BITUMEN-CONCRETE MIXTURE ON NANO-MODIFIED BINDER | 2013 |
|
RU2521988C1 |
Authors
Dates
2014-05-20—Published
2012-11-07—Filed