FIELD: process engineering.
SUBSTANCE: invention relates to production of spherical powders for small arms. Proposed method consists in production of powder varnish in reactor, dispersing into spherical particles, dewatering and distillation of ethyl acetate from spherical powder followed by its flushing, sorting and drying. Note here spherical powder with graphite is fed via settling cyclone into drying chamber with blow-out surface. Powder drying is conducted under boiling conditions at air pressure in drying chamber created by screens arranged at chamber bottom. Heat carrier is fed to chamber bottom part for 60-80 minutes at 88-98°C, then 140-180 minutes at 65-75°C and for 20-30 minutes at 50-60°C. Dried powder is discharged into intake bin and forced by air for dry sorting.
EFFECT: spherical powder moisture content complying with preset powder characteristics.
1 dwg, 1 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING SPHERICAL POWDER | 2012 |
|
RU2497789C1 |
DRYING METHOD OF PELLET POWDER | 2014 |
|
RU2598091C2 |
METHOD OF DRYING SPHERICAL POWDER | 2015 |
|
RU2622134C2 |
METHOD OF PRODUCING PELLET POWDER FOR SMALL ARMS | 2015 |
|
RU2593451C1 |
METHOD FOR SPHERICAL GUN POWDER GRAPHITIZATION | 2015 |
|
RU2597317C2 |
METHOD OF SPHERICAL POWDER PRE-DRYING | 2012 |
|
RU2497792C1 |
METHOD OF MAKING SPHERICAL POWDER FOR SMALL ARMS | 2012 |
|
RU2525544C2 |
METHOD OF SPHERICAL POWDER GRAPHITISATION | 2010 |
|
RU2456257C2 |
METHOD OF SPHERICAL GUNPOWDER RETARDING | 2012 |
|
RU2497788C1 |
METHOD OF PRODUCTION OF SPHERICAL POWDER FOR SHOT CARTRIDGES FOR SMOOTH-BORE SPORTS AND HUNTING WEAPONS OF 12, 16 AND 20 CALIBRE | 2012 |
|
RU2522642C2 |
Authors
Dates
2014-05-20—Published
2012-03-05—Filed