FIELD: metallurgy.
SUBSTANCE: proposed composition contains the following substances, in wt %: soda - 19.0-21.0, borax - 5.0-7.0, cryolite - 5.0-7.0, perlite and/or obsidian - 67.0-69.0. Glass melting is performed at 1260-1300°C. Melt is poured in metal moulds made from refractory steel. Glass articles are subjected to annealing and machining.
EFFECT: lower temperature glass melting.
1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| MIXTURE FOR PRODUCING COLOURED GLASS | 2012 |
|
RU2495838C1 |
| MIXTURE FOR MAKING GLASS | 2011 |
|
RU2465226C1 |
| CHARGE FOR OBTAINING COLOURED GLASS | 2008 |
|
RU2365545C1 |
| GLASE COMPOSITION | 2010 |
|
RU2417205C1 |
| MIXTURE FOR PRODUCING COLOURED GLASS | 2010 |
|
RU2424992C1 |
| CHARGE FOR GLASS PRODUCTION | 2011 |
|
RU2469964C1 |
| MIXTURE FOR PRODUCING COLOURED GLASS | 2011 |
|
RU2465227C1 |
| MIXTURE FOR PRODUCING COLOURED GLASS | 2011 |
|
RU2465228C1 |
| CHARGE COMPOSITION OF GLAZE | 2013 |
|
RU2526091C1 |
| MIXTURE FOR MAKING GLASS | 2010 |
|
RU2417165C1 |
Authors
Dates
2014-05-27—Published
2013-04-17—Filed