FIELD: metallurgy.
SUBSTANCE: proposed alloy contains the following components in wt %: chromium - 9-16, cobalt 10-16, tungsten 4-9, molybdenum - 0.2-3.0, aluminium - 1.8-4.5, titanium 2.0-4.5, tantalum - 2.5-7.0, niobium 0.01-1.5, boron 0.01-0.5, lanthanum 0.01-0.5, yttrium 0.01-0.2, cerium 0.01-0.2, rhenium - 0.5-5.0, hafnium 0.1-1.0, manganese 0.05-1.0, silicon - 0.05-1.0, magnesium 0.01-0.2, nickel making the rest.
EFFECT: higher resistance to sulphide corrosion, heat resistance.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
CASTING NICKEL ALLOY WITH INCREASED HEAT STRENGTH AND RESISTANCE TO SULFIDE CORROSION | 2015 |
|
RU2623940C2 |
HEAT-RESISTANT ALLOY ON NICKEL BASIS FOR MONOCRYSTALLINE CASTING | 2011 |
|
RU2465359C1 |
DEFORMABLE NICKEL-BASED HEAT-RESISTANT ALLOY | 2019 |
|
RU2695097C1 |
CAST CORROSION-RESISTANT NICKEL-BASED POLYCRYSTALLINE SUPERALLOY | 2022 |
|
RU2803779C1 |
CAST HEAT-RESISTANT NICKEL ALLOY WITH MONOCRYSTALLINE STRUCTURE | 2021 |
|
RU2768946C1 |
HEAT-RESISTANT ALLOY ON NICKEL BASIS FOR MONOCRYSTALLINE CASTING | 2010 |
|
RU2439184C1 |
CAST HEAT-RESISTANT NICKEL ALLOY WITH MONOCRYSTALLINE STRUCTURE | 2021 |
|
RU2769330C1 |
COMPOSITION OF HEAT-RESISTANT NICKEL ALLOY (VERSIONS) | 2007 |
|
RU2353691C2 |
NICKEL-BASED CASTING HEAT RESISTANT ALLOY | 1994 |
|
RU2081930C1 |
HEAT-RESISTANT NICKEL ALLOY | 2019 |
|
RU2697674C1 |
Authors
Dates
2014-06-27—Published
2013-03-15—Filed