FIELD: chemistry.
SUBSTANCE: method of obtaining uranium dioxide consists in hydration of metal uranium at a temperature of 200-220°C, dehydration at a temperature of 470-500°C and oxidation at a temperature of 600-800°C in a flow of a mixture of hydrogen and water vapours in a ratio 40:1-1.2 (molar parts).
EFFECT: increased dispersity and specific surface of an uranium dioxide powder, obtaining uranium dioxide with oxygen coefficient close to stoichiometric one, reduction of the process duration.
2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
PRODUCTION OF URANIUM NITRIDE POWDERS | 2013 |
|
RU2522814C1 |
METHOD OF TESTING FOR COMPATIBILITY OF NUCLEAR FUEL POWDER WITH MATERIAL OF FUEL ELEMENT CLADDING | 2015 |
|
RU2581846C1 |
CATALYST AND METHOD OF DEHYDROGENATING HYDROCARBONS IN PRESENCE OF SAID CATALYST | 2008 |
|
RU2394642C1 |
METHOD OF OXIDATING TREATMENT (VOLOXIDIATION) OF IRRADIATED NUCLEAR FUEL | 2017 |
|
RU2654536C1 |
METHOD OF PROCESSING IRRADIATED NUCLEAR FUEL | 2015 |
|
RU2591215C1 |
METHOD FOR PREPARING URANIUM DIOXIDE POWDER-BASE TABLETTED FUEL | 2004 |
|
RU2296106C2 |
URANIUM HEXAFLUORIDE CONVERSION METHOD | 1998 |
|
RU2203225C2 |
METHOD OF PRODUCING URANIUM OXIDE | 2015 |
|
RU2603359C1 |
METHOD OF OBTAINING URANIUM DIOXIDE POWDER | 2013 |
|
RU2542317C2 |
METHOD OF PRODUCING SOLID PLUTONIUM DIOXIDE SOLUTION IN URANIUM DIOXIDE MATRIX | 2013 |
|
RU2554626C2 |
Authors
Dates
2014-07-20—Published
2013-01-09—Filed