FIELD: chemistry.
SUBSTANCE: invention relates to a method of obtaining mineral silicic water (MSW), intended for application for medical purposes. The method of obtaining includes hydrolysis of tetraethoxysilane in the TEOS mixture: ethanol: water, acidified by HCl. Nanosol is obtained at a temperature of 55-65°C for 1.5 hours with evaporation of ethanol to the volume reduction by 1/3, then, dilution of the obtained nanosol with a physiological solution NaCl is carried out in 2 steps with equal portions of the physiological solution, preliminarily heated to 40-50 in a ratio of volumes of the initial nanosol: physiological solution 1:7 with 15-minute interval. After each dilution a temperature of the solution is kept in the range of 55-65°C.
EFFECT: increase of the compound application efficiency.
1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF YEAST ACTIVATION | 2012 |
|
RU2492230C1 |
METHOD TO PRODUCE NANOPARTICLES OF SILICA | 2010 |
|
RU2426692C1 |
METHOD TO PRODUCE MODIFIED OPTICAL CHEMOSENSORY FILMS BASED ON SILICA | 2010 |
|
RU2433084C1 |
METHOD FOR NOBLE OPAL PRODUCTION | 0 |
|
SU1807976A3 |
METHOD FOR PRODUCTION OF COMPOSITE OPTICAL CHEMOSENSOR FILM | 2009 |
|
RU2399585C1 |
METHOD FOR PRODUCTION OF COMPOSITE OPTICAL CHEMOSENSOR FILMS | 2009 |
|
RU2399584C1 |
METHOD OF REINFORCING PHOTONIC-CRYSTALLINE FILMS BASED ON MONODISPERSED SPHERICAL SILICA PARTICLES | 2008 |
|
RU2399586C1 |
METHOD OF OBTAINING CHEMOSENSORY FILMS | 2008 |
|
RU2370310C1 |
METHOD FOR PRODUCTION OF PHOTON-CRYSTALLINE OPAL FILMS | 2008 |
|
RU2389683C2 |
METHOD OF PRODUCING ANTIREFLECTION MESOPOROUS SILICON DIOXIDE-BASED COATINGS | 2014 |
|
RU2564710C1 |
Authors
Dates
2014-07-20—Published
2013-07-05—Filed