FIELD: mining.
SUBSTANCE: bore mud is mixed with sand at the ratio of 1:(0.75-5) to add hydrochloric acid in amount of 0.02-2.246 gram-molecules per 1 kg of mud to mix pH of 5 to 8, mix being mixed and dried thereafter. As a result, inert construction material or man-caused soil is produced from wastes. To select more accurate recipe, bore mud is subjected to analysis for content of clay particles and pH level.
EFFECT: simple and reliable process.
6 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
TECHNOGENIC SOIL | 2019 |
|
RU2725534C1 |
METHOD FOR DISPOSING DRILLING MUD WHEN PRODUCING MAN-MADE SOIL | 2017 |
|
RU2631681C1 |
CONSTRUCTION MATERIAL RESOIL | 2015 |
|
RU2593289C1 |
METHOD FOR DRILLING MUD CONDITIONING | 2018 |
|
RU2690254C1 |
MAN-MADE SOIL OBTAINED BY THERMAL TREATMENT FOR RECLAMATION OF DISTURBED LANDS | 2013 |
|
RU2520146C1 |
WELL DRILLING WASTE UTILISATION METHOD | 2010 |
|
RU2425815C1 |
METHOD FOR THE DISPOSAL OF DRILLING MUDS WITH THE PRODUCTION OF ENVIRONMENTALLY FRIENDLY SOIL | 2017 |
|
RU2661831C1 |
METHOD FOR PROCESSING DRILL CUTTINGS TO OBTAIN RECLAMATION SOIL FOR TECHNICAL AND BIOLOGICAL RECLAMATION | 2022 |
|
RU2802741C1 |
UNIVERSAL METHOD OF COMPLEX WELL-DRILLING WASTE NEUTRALIZATION TO PRODUCE ANTHROPOGENIC REINFORCED SOIL (ARS) BUILDING COMPOSITE | 2015 |
|
RU2616304C1 |
SOIL-SLIME MIX | 2013 |
|
RU2522317C1 |
Authors
Dates
2014-08-10—Published
2013-02-19—Filed