FIELD: metallurgy.
SUBSTANCE: proposed method comprises preparation of charge by mixing the tinstone concentrate with coal and fluxing additives consisting of sodium carbonate and sodium chloride and reduction melting of said charge at 870°C. Then, obtained melt is cooled to separate metal from slag. Note here that charge melt is irradiated by nanosecond electromagnetic pulses for 10-30 minutes.
EFFECT: higher yield of lead, accelerated melting.
1 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
PROCEDURE FOR PRODUCTION OF TIN OUT OF KASSITERIT CONCENTRATE | 2009 |
|
RU2393252C1 |
METHOD OF TIN MANUFACTURING FROM CASSITERITE CONCENTRATE | 2006 |
|
RU2333268C2 |
COPPER GALVANIC SLUDGE PROCESSING METHOD | 2013 |
|
RU2535110C1 |
ELECTRIC ARC METHOD FOR PRODUCING OF FIRST-GRADE TIN (ALLOY WITH COMPOSITION APPROXIMATING THAT OF 04 GRADE) FROM CASSITERITE CONCENTRATE | 2002 |
|
RU2224037C2 |
METHOD OF ALUMINIUM ALLOYS TREATMENT | 2013 |
|
RU2546948C1 |
MELT COPPER AND ITS ALLOYS TREATMENT PROCESS WITH USE OF NANOSECOND ELECTROMAGNETIC PULSES FOR INCREASING HEAT CONDUCTANCE OF MELT | 2005 |
|
RU2287605C1 |
METHOD OF GREY CAST IRON TREATMENT BY NANO-SECOND ELECTRO-MAGNETIC PULSES (NEMP) FOR IMPROVING HEAT CONDUCTIVITY, CORROSION STABILITY AND HEAT RESISTANCE | 2007 |
|
RU2354496C2 |
METHOD OF TREATMENT OF LIQUID ALUMINIUM AND SILUMIN WITH NANO-SECOND ELECTRO-MAGNETIC IMPULSES (NEMI) TO UPGRADE THEIR THERMO-CONDUCTIVITY | 2007 |
|
RU2347643C1 |
CAST-IRON MELT PROCESSING METHOD BY NANOSECOND ELECTROMAGNETIC IMPULSES (NEMI) | 2016 |
|
RU2623390C1 |
METHOD FOR PRODUCING POWDERS OF MOLYBDENUM OR ITS COMPOSITES WITH TUNGSTEN | 2005 |
|
RU2285586C1 |
Authors
Dates
2014-09-10—Published
2013-05-06—Filed