FIELD: metallurgy.
SUBSTANCE: foaming mix is placed in metal moulds to be heated in the furnace at the rate of 3.7°C/min to 820°C with holding for 40 min with subsequent sharp cooling to 600°C at the rate of 2.0°C/min and annealing for 12 hours.
EFFECT: higher heat resistance and hardness of finished product, lower power input, accelerated annealing.
4 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF OBTAINING BLOCK TEMPERATURE-RESISTANT FOAM GLASS | 2013 |
|
RU2536543C1 |
METHOD OF PRODUCING BLOCK HEAT-RESISTANT FOAM GLASS | 2019 |
|
RU2730236C1 |
METHOD OF PRODUCING BLOCK HEAT-RESISTANT FOAMED GLASS | 2014 |
|
RU2556584C1 |
RAW MIX FOR MANUFACTURING OF BLOCK FOAM GLASS AND METHOD OF ITS MANUFACTURING | 2014 |
|
RU2570175C1 |
METHOD FOR PRODUCTION OF FOAM GLASS | 2008 |
|
RU2351554C1 |
METHOD OF PRODUCING COATING ON BLOCK FOAM GLASS | 2019 |
|
RU2726015C1 |
METHOD OF PRODUCING HEAT-INSULATION FACING MATERIAL BASED ON FOAMED GLASS | 2011 |
|
RU2485058C1 |
METHOD FOR PRODUCTION OF THERMAL INSULATION BOARDS FROM FOAM GLASS BASED ON CULLET | 2022 |
|
RU2781293C1 |
METHOD OF PRODUCING FOAMGLASS | 0 |
|
SU1673544A1 |
BLEND FOR PREPARING FOAM GLASS | 1998 |
|
RU2149146C1 |
Authors
Dates
2014-10-10—Published
2013-07-02—Filed