FIELD: metallurgy.
SUBSTANCE: mix contains quartz sand 82-85 wt %, refractory clay or bentonite 5-8 wt %, 6-8% water solution of styromal 5-8 wt %, dextrin 2-2.5 wt % and water 2-5 wt %.
EFFECT: higher strength of the mix in 30-40 minutes after preparation, higher quality of finished casts.
2 cl, 2 ex