FIELD: metallurgy. SUBSTANCE: mixture has the following components, wt. -%: depleted sand-clay mixture 38.0-47.0; water-glass binding agent 4.2-4.4; aluminium hydroxide 0.20-0.25; sodium hydroxide 0.50-0.55; technical water 0.60-0.80 and silicon dioxide-base refractory filling agent - the rest. Mixture can be used for making casting forms and rods solidified by heat drying. EFFECT: decreased consumption of pure refractory filling agent, unusing molding clay, improved knocking-out, retained necessary strength after hardening, decreased collapsibility mixture. 5 tbl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
MIX FOR MANUFACTURING MOLDS AND RODS (VERSIONS) | 1999 |
|
RU2151018C1 |
ANTIPENETRATION WASH FOR MOLDS AND RODS | 1999 |
|
RU2151019C1 |
SUSPENSION FOR MANUFACTURING CERAMIC MOLDS AND MOLD CORES | 1999 |
|
RU2152841C1 |
MIXTURE FOR MAKING CASTING MOLDS AND CORES | 0 |
|
SU1775211A1 |
MIXTURE FOR MAKING MOLDS AND RODS | 2019 |
|
RU2703637C1 |
SUSPENSION FOR PRODUCTION OF SHELL MOLDS IN INVESTMENT CASTING | 1998 |
|
RU2130358C1 |
METHOD FOR MAKING CASTING MOLDS AND CORES FROM LIQUID GLASS MIXTURES | 1998 |
|
RU2145265C1 |
GLASS-CUBES MIXTURE FOR MAKING MOLDS AND RODS AND METHOD FOR ITS PREPARATION | 2017 |
|
RU2688322C1 |
MIX FOR PREPARING MOULDS AND CORES | 0 |
|
SU1069922A1 |
MIXTURE FOR MANUFACTURE OF CASTING MOLDS AND CORES | 1997 |
|
RU2167021C2 |
Authors
Dates
2000-05-10—Published
1999-06-21—Filed