FIELD: construction.
SUBSTANCE: polymer binding agent contains polyester resin based on polyethyleneglycol maleate phthalate, a hardening agent - cobalt naphthenate, and as a hardening initiating agent - methylethylketone peroxide in a dimethyl phtalate solution, at the following component ratio (wt %): polyester resin based on polyethyleneglycol maleate phthalate 95.7-97.48, cobalt naphthenate 0.75-1.75, methylethylketone peroxide in dimethyl phtalate is the rest.
EFFECT: increasing strength properties of a polymer binding agent and polymer concretes on its basis.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
POLYMER BINDING AGENT FOR POLYMER CONCRETE | 2013 |
|
RU2550872C2 |
POLYMER-MINERAL SOLUTION FOR IMPREGNATING FRAME MADE OF MINERAL AGGREGATE | 2013 |
|
RU2529681C1 |
POLYMER-CONCRETE MIXTURE | 2010 |
|
RU2417178C1 |
POLYMER-MINERAL SOLUTION FOR IMPREGNATION OF FRAME FROM MINERAL FILLER | 2010 |
|
RU2429266C1 |
POLYESTER COMPOSITION | 2015 |
|
RU2577284C1 |
POLYMER-MORTAR MIXTURE | 2010 |
|
RU2417962C1 |
POLYMER COMPOSITION | 2002 |
|
RU2270217C2 |
DECORATIVE BOARD BASED ON VENEER | 2014 |
|
RU2541003C1 |
COMPOSITION FOR HYDROINSULATING, ANTI-CORROSIVE AND SEALING COATING | 2005 |
|
RU2291175C1 |
NANOMODIFIED POLYMER COMPOSITE | 2012 |
|
RU2488563C1 |
Authors
Dates
2014-12-10—Published
2013-09-25—Filed