FIELD: chemistry.
SUBSTANCE: polymer-mineral solution for impregnating a frame made of a mineral aggregate, which includes polyether acrylate resin, a hardening initiator, a hardening accelerator and an additive, the hardening initiator being cyclohexanone peroxide, the hardening accelerator being cobalt octoate and the additive being a mixture of quartz filling materials having two particle sizes of 0.071-0.16 mm and 0.16-0.315 mm in ratio of 3:1, said impregnation being carried out by filling voids in the hardened frame with said solution, said frame being obtained by moulding a mixture of the following composition, wt %: polyether acrylate resin 6.0, cyclohexanone peroxide 0.12, cobalt octoate 0.28, granite chips with size of 5-8 mm 93.6, with the following ratio of components, wt %: polyether acrylate resin 24-28, cyclohexanone peroxide 0.48-0.56, cobalt octoate 1.1-1.29, mixture of quartz filling materials having two particle sizes 0.071-0.16 and 0.16-0.315 in ratio of 3:1 - the balance.
EFFECT: improved strength properties.
3 tbl
Title | Year | Author | Number |
---|---|---|---|
POLYMER BINDING AGENT FOR POLYMER CONCRETE | 2013 |
|
RU2550872C2 |
POLYMER-MINERAL SOLUTION FOR IMPREGNATION OF FRAME FROM MINERAL FILLER | 2010 |
|
RU2429266C1 |
POLYMER-MINERAL SOLUTION FOR IMPREGNATION OF THE FRAMEWORK MADE OUT OF MINERAL FILLER | 2004 |
|
RU2276122C2 |
POLYMER BINDING AGENT FOR POLYMER CONCRETE | 2013 |
|
RU2534692C1 |
POLYMERIC CONCRETE MIX | 0 |
|
SU996378A1 |
POLYMER-MINERAL SOLUTION FOR IMPREGNATION OF SKELETON OF MINERAL FILLER | 1998 |
|
RU2131855C1 |
POLYMER-MINERAL MORTAR | 0 |
|
SU1754688A1 |
POLYMER-CONCRETE MIXTURE | 2010 |
|
RU2417178C1 |
METHOD FOR MANUFACTURING POLYMER CONCRETE MACHINE BASE | 2023 |
|
RU2813041C1 |
POLYMER-CONCRETE MIXTURE | 0 |
|
SU1701686A1 |
Authors
Dates
2014-09-27—Published
2013-06-18—Filed