FIELD: chemistry.
SUBSTANCE: in a method of producing a porous aggregate, which includes preparation of a ceramic casting mixture, immersing aggregate particles into the mixture, drying said particles and firing, drying is carried out to moisture content of no more than 6%, firing is carried out at temperature of 850-1200°C and the aggregate used is natural vermiculite with particle size of 5-10 mm, wherein the mixture has the following composition, wt %: natural vermiculite 20-25, clay 24-30, water 45-50, colouring additive1-5. The method includes impregnating the porous aggregate with sodium ethyl siliconate or sodium methyl siliconate, followed by drying.
EFFECT: obtaining a light-weight, high-strength decorative porous aggregate.
2 cl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD TO PRODUCE POROUS FILLER | 2014 |
|
RU2561386C1 |
METHOD OF PRODUCING POROUS AGGREGATE | 2013 |
|
RU2510370C1 |
METHOD OF PRODUCING POROUS AGGREGATE | 2012 |
|
RU2481281C1 |
METHOD OF PRODUCING POROUS AGGREGATE | 2011 |
|
RU2484033C1 |
METHOD OF PRODUCING POROUS AGGREGATE | 2011 |
|
RU2481288C1 |
METHOD OF PRODUCING POROUS AGGREGATE (VERSIONS) | 2011 |
|
RU2439013C1 |
METHOD OF PRODUCING POROUS AGGREGATE | 2010 |
|
RU2449961C1 |
CERAMIC MIXTURE FOR MAKING BRICKS | 2017 |
|
RU2648126C1 |
FURNACE CHARGE FOR POROUS FILLER PRODUCTION | 2014 |
|
RU2562072C1 |
METHOD OF MANUFACTURING POROUS FILLING AGENT | 2011 |
|
RU2473489C1 |
Authors
Dates
2015-01-10—Published
2013-12-12—Filed