FIELD: chemistry.
SUBSTANCE: silicate pain contains thermolysis defecate - waste of sugar production - annealed at temperature 260 and 600°C, with particle size 1-2 mcm. Silicate paint includes, wt. p.: zinc dry white - 15-55, talc -15, defecate, annealed at temperature 600°C, - 10-64, defecate, annealed at temperature 260°C, - 12-63. Liquid sodium or potassium glass with density not less than 1200 kg/m3 is used with weight ratio 1:1 relative to dry part of paint. Paint contains pigment of red colour, obtained from tailings of dressing of ferruginous quartzites - TDFQ, annealed at temperature 1000°C.
EFFECT: improvement of painting and technical parameters.
2 cl, 3 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
SILICATE COATING WITH INCREASED DURABILITY AND METHOD OF ITS PREPARATION | 2017 |
|
RU2669642C2 |
COMPOSITE SILICATE PAINT | 2016 |
|
RU2645502C2 |
COMPOSITE SILICATE PAINT | 1996 |
|
RU2160753C2 |
METHOD OF PREPARING OF BUILDING SILICATE DYE | 1992 |
|
RU2034810C1 |
SILICATE PAINT | 0 |
|
SU823402A1 |
SILICATE PAINT | 0 |
|
SU939504A1 |
COATING COMPOSITION | 0 |
|
SU1031997A1 |
SILICATE PAINT | 0 |
|
SU767154A1 |
ONE-POT SILICATE PAINT | 2005 |
|
RU2294947C1 |
SILICATE BUILDING PAINT | 2005 |
|
RU2294946C1 |
Authors
Dates
2015-02-10—Published
2013-07-11—Filed