FIELD: chemistry.
SUBSTANCE: invention can be used in production of scintillation ceramics with increased light output. Method of obtaining barium fluoride powder, activated with cerium fluoride, includes interaction of ammonium fluoride solution with solution, containing barium nitrate and cerium nitrate. For interaction used is solution, containing barium and cerium ions with their molar ratio from 99.999:0.001 to 99.990:0.010, respectively. After that, sediment is separated, washed, dried and subjected to thermal processing at temperature 550-600°C. Washed residue is re-processed with highly pure hydrofluoric acid.
EFFECT: invention makes it possible to obtain finely disperse water-free powder of barium fluoride, activated with cerium fluoride, with homogeneous chemical and phase composition and low content of activator, hydrogen and carbon admixtures.
3 cl, 9 dwg, 2 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR OBTAINING STRONTIUM FLUORIDE POWDER, ACTIVATED WITH NEODYMIUM FLUORIDE, FOR LASER CERAMICS | 2014 |
|
RU2574264C1 |
METHOD FOR SYNTHESIS OF MONOPHASE BARIUM FLUORIDE NANOPOWDER DOPED WITH FLUORIDE OF RARE-EARTH METAL | 2009 |
|
RU2411185C1 |
METHOD OF PRODUCING HIGH-PURITY BARIUM FLUORIDE | 2009 |
|
RU2424187C1 |
LASER FLUORIDE CERAMICS AND ITS PRODUCTION PROCESS | 2006 |
|
RU2321120C1 |
METHOD OF PRODUCING HIGH-PURITY CALCIUM FLUORIDE | 2009 |
|
RU2424188C1 |
METHOD FOR PRODUCING METAL FLUORIDES | 2006 |
|
RU2328448C1 |
METHOD OF PRODUCING FLUORIDE NANOCERAMIC | 2010 |
|
RU2436877C1 |
METHOD OF PRODUCING HIGH-PURITY STRONTIUM FLUORIDE | 2009 |
|
RU2424189C1 |
METHOD OF PRODUCING HIGH-PURITY ANHYDROUS POLYCRYSTALLINE CERIUM FLUORIDE | 1996 |
|
RU2107029C1 |
LASER FLUORIDE NANOCERAMIC AND METHOD FOR PRODUCTION THEREOF | 2011 |
|
RU2484187C1 |
Authors
Dates
2015-03-27—Published
2013-06-27—Filed