FIELD: chemistry.
SUBSTANCE: invention can be used in chemical and electronic industry. The volume per particle of α-aluminium oxide for producing monocrystalline sapphire is not less than 0.01 cm3, relative density is not less than 80%, bulk density of the aggregate is 1.5-2.3 g/cm3, and its shape is any one of spherical, cylindrical and briquette-like.
EFFECT: invention reduces the amount of adsorbed water, reduces crucible oxidation and improves the efficiency of producing monocrystalline sapphire.
3 cl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
α-ALUMINUM OXIDE POWDER | 2007 |
|
RU2441841C2 |
ALUMINIUM α-OXIDE FOR OBTAINING SAPPHIRE MONOCRYSTAL AND METHOD OF OBTAINING THEREOF | 2011 |
|
RU2554196C2 |
METHOD OF PREPARING ALPHA-ALUMINUM POWDER AND ALPHA-ALUMINUM POWDER | 1994 |
|
RU2136596C1 |
SINTERED BODY FROM ALPHA-ALUMINA FOR PRODUCING SAPPHIRE SINGLE CRYSTAL | 2011 |
|
RU2579596C2 |
ALUMINUM OXIDE | 1993 |
|
RU2107661C1 |
METHOD FOR PRODUCING ALPHA-ALUMINIUM OXIDE FOR SUBSEQUENT GROWTH OF SINGLE-CRYSTAL SAPPHIRE | 2020 |
|
RU2742575C1 |
METHOD OF ALUMINIUM α-OXIDE PRODUCING (VARIANTS) | 1993 |
|
RU2114059C1 |
α---ALUMINA POWDER AND A METHOD OF ITS PRODUCING | 1994 |
|
RU2118612C1 |
POWDER OF METAL OXIDE, POWDER OF TITANIUM OXIDE, METHOD OF PRODUCING METAL OXIDE POWDER | 1994 |
|
RU2127221C1 |
ALUMINUM OXIDE | 1993 |
|
RU2107662C1 |
Authors
Dates
2015-06-10—Published
2010-11-19—Filed