FIELD: chemistry.
SUBSTANCE: polycarbonate pyrolysis is carried out in a medium of coal-tar pitch with a ratio of polycarbonate: coal-tar pitch, equal (1.5-4.0):10.0 in an interval of temperatures of 350-380°C. A solid residue of the pyrolysis is subjected to chemical activation by its thermal processing in a mixture with an alkali metal hydroxide.
EFFECT: increased output of the product with high sorption characteristics.
1 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING PITCH FROM WASTE FRACTIONATION OF STILL RESIDUE OF STYRENE | 2018 |
|
RU2687899C2 |
METHOD OF PROCESSING WASTES CONTAINING THERMOSETTING POLYMERS | 2015 |
|
RU2600637C2 |
METHOD OF RECYCLING FILLER FROM WASTES OF POLYMER COMPOSITE MATERIALS (PCM) | 2020 |
|
RU2734676C1 |
METHOD FOR PRODUCING ACTIVATED CARBON | 2015 |
|
RU2582132C1 |
METHOD OF OBTAINING CARBON ADSORBENT | 2012 |
|
RU2518579C1 |
METHOD OF OBTAINING GRANULATED ACTIVE CARBON | 2006 |
|
RU2331580C1 |
METHOD OF PRODUCING CARBON-BASED SORBENT | 2013 |
|
RU2565194C2 |
METHOD OF PRODUCING BINDER FOR MAKING CARBON MATERIALS AND ARTICLES THEREFROM | 2015 |
|
RU2586139C1 |
METHOD TO PRODUCE CARBON ADSORBENT | 2010 |
|
RU2436625C1 |
METHOD FOR PRODUCING OIL PITCH | 2020 |
|
RU2750991C1 |
Authors
Dates
2015-07-10—Published
2014-01-09—Filed