FIELD: chemistry.
SUBSTANCE: invention relates to methods of obtaining sulphur concretes for application in manufacturing building constructions and production of construction products, subjected to acid and salt aggression. Composition for sulphur concretes, containing sulphur binding agent and inert filler, is characterised by the fact that sulphur binding agent is obtained by mixing at temperature 135°C in vortex mixing apparatus for 45-60 sec sulphur with addition of black oil in weight ratio 6:1 and spraying ammonia and fumaric acid in amount 200 mg per 1 m3 of sulphur respectively, until homogeneous mixture is obtained, with inert filling agent containing the following fraction composition in wt %: screenings of rubble crushing - fraction 20-10 mm - 10, fraction 10-5 mm - 10, fraction 5-2.5 mm - 10; washed river sand - fraction 2.5-1.25 mm - 10, fraction 1.25-0.63 mm - 15, fraction 0.63-0.315 mm - 15, fraction 0.315-0.071 mm - 15; grinding of washed river sand - fraction 0.071 mm and smaller - 15. To obtain composition sulphur binding agent and inert filler can be used in weight ratio 23:77.
EFFECT: increased strength and fire resistance of concrete.
2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR SULFUR CONCRETES | 2007 |
|
RU2356867C1 |
COMPOSITE MIXTURE FOR PRODUCING SULPHUR CONCRETE | 2023 |
|
RU2800504C1 |
SULPHUR CONCRETE COMPOSITION | 2012 |
|
RU2521986C1 |
CONCRETE MIX | 0 |
|
SU1601088A1 |
SULPHUR CONCRETE COMPOSITION | 2010 |
|
RU2448924C2 |
RAW MIX FOR MANUFACTURING BUILDING PRODUCTS AND STRUCTURES | 2000 |
|
RU2177923C2 |
SULPHUR CONCRETE MIX AND METHOD OF ITS PRODUCTION | 2010 |
|
RU2430053C1 |
SULFUR BINDER AND SULFUR/CONCRETE MIX | 2005 |
|
RU2306285C2 |
COMPOSITION FOR CIVIL ENGINEERING WORK | 1996 |
|
RU2074141C1 |
RAW MATERIAL MIXTURE FOR SULFUR CONCRETE AND METHOD OF ITS PREPARING | 2016 |
|
RU2626083C1 |
Authors
Dates
2015-11-10—Published
2013-12-10—Filed