FIELD: chemistry.
SUBSTANCE: in method of obtaining activated reinforced mineral powder for asphalt concrete mixture mineral component in form of carbonate rock, water-repelling agent - fatty acid with melting temperature not higher than 85°C, reinforcing additive in form of fibres are milled together in centrifugal mill with the following component ratio, wt %: said water-repellent 0.1-5.0; fibres 0.5-15.0; carbonate rock - the remaining part. Activated reinforced mineral powder for asphalt-concrete mixture contains homogenous mixture of milled mineral component in form of carbonate rock, mainly of cubical shape, reinforcing additive in form of loosed fibres and water-repellent in form of fatty acid, uniformly distributed on the surface of mineral component and reinforcing additive, with the following component ratio, wt %: said water-repellent 0.1-5.0, fibres 0.5-15.0; carbonate rock - the remaining part. Invention is developed in dependent items.
EFFECT: technology simplification, improvement of exploitation characteristics, increase of ecologically safety.
8 cl, 1 tbl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
PETROLEUM COKE FOR AN ASPHALT CONCRETE MIXTURE | 2020 |
|
RU2754902C1 |
ACTIVATED MINERAL POWDER FOR ROAD CONCRETE MIX AND METHOD FOR MANUFACTURING THEREOF | 2017 |
|
RU2671227C1 |
MINERAL POWDER FOR ASPHALT-CONCRETE MIXTURE (VERSIONS) | 2019 |
|
RU2715403C1 |
METHOD FOR REINFORCEMENT OF ASPHALT CONCRETE MIX | 2006 |
|
RU2351561C2 |
ASPHALT MIX AND METHOD FOR PREPARATION THEREOF | 2011 |
|
RU2465231C1 |
METHOD FOR PREPARING MINERAL POWDER | 2017 |
|
RU2662829C1 |
METHOD OF REINFORCING ASPHALT-CONCRETE MIX | 2003 |
|
RU2262491C2 |
POLYMERIC-BITUMINOUS BINDING AND THE ASPHALT-CONCRETE MIXTURE PREPARED ON ITS BASIS | 2006 |
|
RU2297990C1 |
ASPHALT CONCRETE MIXTURE | 2000 |
|
RU2204537C2 |
MINERAL POWDER FOR ASPHALT CONCRETE MIXTURE | 2012 |
|
RU2515277C1 |
Authors
Dates
2015-11-20—Published
2014-10-22—Filed