FIELD: construction.
SUBSTANCE: concrete mix, containing portland cement, sand, crushed stone, water, modifying additive - plasticiser, and shale ash produced by burning of flammable dispersed shales on heat power plants with shale ash particle size of 9-12 micron, contains 6-16% of free calcium oxide, 27.0-34.0 wt % of glassy phase and 15.0-35.0 wt % of insoluble residue, and specific surface of shale ash makes 2800-5000 cm2/g, and content of chlorides in it of 0.01-0.6 wt %, at the following ratio of specified components, wt %: portland cement 7.00-21.09, crushed stone 40.00-46.41, sand 30.00-39.60 or 41.00-46.60, shale ash 2.10-8.43, modifying additive 0.01-6.00, water - balance.
EFFECT: development of a concrete mix with improved physical-mechanical properties, making it possible to produce concrete with improved operational characteristics, including lower subsidence.
2 ex
Title | Year | Author | Number |
---|---|---|---|
CONCRETE MIX | 2023 |
|
RU2804035C1 |
CONCRETE MIXTURE | 2016 |
|
RU2632082C1 |
CONCRETE MIXTURE | 2010 |
|
RU2433973C1 |
CONCRETE MIXTURE | 2013 |
|
RU2525565C1 |
CONCRETE MIX AND METHOD OF PREPARATION OF SUCH MIX | 2006 |
|
RU2307810C1 |
HIGH-STRENGTH CONCRETE | 2012 |
|
RU2515250C1 |
HIGH-STRENGTH CONCRETE | 2010 |
|
RU2433098C1 |
CONCRETE MIX | 0 |
|
SU1038311A1 |
CONCRETE MIXTURE | 2009 |
|
RU2439020C2 |
HIGH-STRENGTH CONCRETE | 2014 |
|
RU2579837C1 |
Authors
Dates
2015-11-27—Published
2014-07-31—Filed