FIELD: construction.
SUBSTANCE: wood-marble-cement mixture to manufacture heat insulating and structural construction materials contains polypropylene fibres with length 8-30 mm and diameter 0.08-0.3 mm as nonorganic addition, and marble is used with particles size 10 mcm maximum, including up to 0.02% of particles with size below 0.5 mcm, including nanoparticles, at the following ratio of components, wt %: Portland cement 38-39, construction killed hydrated lime 4-5, softwood sawdust 43.6-45.6, micro marble 4-5, liquid glass 6-7.5, calcium chloride 2.3-4.3, polypropylene fibres 0.1-0.2, at that water additives to the said mixture is made to receive water-cement ratio 0.8-1.2.
EFFECT: increased strength and ecological properties of material out of suggested mixture.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
WOOD-TALCUM PEACH-CEMENT MIXTURE | 2014 |
|
RU2570214C1 |
WOOD-CEMENT MIXTURE FOR MAKING BUILDING BLOCKS | 2015 |
|
RU2605110C1 |
WOOD-CEMENT MIX | 2014 |
|
RU2569422C1 |
POLYDISPERSE WOOD-CEMENT MIXTURE WITH NANOMODIFICATOR | 2016 |
|
RU2641349C2 |
WOOD-CEMENT MIXTURE WITH MODIFICATOR | 2016 |
|
RU2641548C2 |
WOOD-CEMENT MIXTURE FOR PRODUCTION OF HEAT-INSULATING AND CONSTRUCTION BUILDING MATERIALS | 2014 |
|
RU2568445C1 |
CONCRETE MIXTURE | 2010 |
|
RU2433974C1 |
RAW MATERIAL MIXTURE FOR PRODUCTION OF PIECE PRODUCTS FROM SAWDUST CONCRETE WITH ADDITION OF FLY ASH | 2012 |
|
RU2570727C2 |
RAW MATERIAL MIXTURE FOR OBTAINING SAWDUST-CONCRETE BRICKS BY METHOD OF SEMI-DRY VIBROCOMPRESSION | 2012 |
|
RU2570726C2 |
COMPOSITION FOR LIGHT-WEIGHT CONSTRUCTION MATERIAL MANUFACTURE | 2008 |
|
RU2376259C1 |
Authors
Dates
2015-12-10—Published
2014-06-17—Filed