FIELD: chemistry.
SUBSTANCE: method is realised by direct interaction in water solution of nickel chloride NiCl2·6H2O with reducing agent of the following formula: , at temperature 90-100°C for 10-15 minutes. Products of interaction are easily separated from water solution. Nickel coating output approaches 100%.
EFFECT: extension of raw material base of reducing agents, elimination of poisonous solutions, simplification of technology.
1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR METAL DEPOSITION ON DIELECTRIC ARTICLES | 0 |
|
SU1315407A1 |
METHOD OF CHEMICAL NICKEL PLATING | 1992 |
|
RU2023749C1 |
APPLICATION OF BIS(4-R-2-AMINOPHENYL) DISULFIDE AS A LEVELING AGENT IN A SOLUTION FOR THE CHEMICAL DEPOSITION OF NICKEL-PHOSPHORUS COATINGS | 2023 |
|
RU2813159C1 |
METHOD FOR COATING COMPOSITE POWDERED MATERIALS | 2013 |
|
RU2556854C2 |
METHOD OF PRODUCING METALLIC MAGNETIC COATINGS | 2018 |
|
RU2710611C1 |
METHOD OF CHEMICAL NICKEL PLATING OF GLASS | 1999 |
|
RU2167113C2 |
METHOD OF PLATING POWDER MATERIALS | 0 |
|
SU821063A1 |
METHOD OF OBTAINING NICKEL (II)-AMMONIUM PHOSPHATES | 2013 |
|
RU2535834C9 |
METHOD OF PREPARING NICKEL COATING ON MATERIALS MADE OF CARBON FIBERS | 1993 |
|
RU2063461C1 |
SOLUTION FOR CHEMICAL PRECIPITATION OF NICKEL-BORON ALLOY | 0 |
|
SU740860A1 |
Authors
Dates
2016-01-20—Published
2014-08-12—Filed