FIELD: construction.
SUBSTANCE: polymer construction material, produced from the mix including polyester resin of Ashlands 280 brand, hardener, filler, where the mix contains as hardener Butanoks M-50, as filler - marble crumb of fraction 0.5-5 mm, and pressed and hardened mix of components is coated by polyurethane varnish, at the following ratio of components, wt %: resin of Ashlands 280 brand 5-7, marble crumb 81-88, polyurethane varnish 5-6, Butanoks M-50 1-7.
EFFECT: increased strength, water impermeability and frost resistance, increased manufacturability of its production.
7 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING HOLLOW LANDSCAPE DECORATIVE ITEMS | 2015 |
|
RU2616020C2 |
POLYMER COMPOSITION FOR FRAMING IMPREGNATION | 2019 |
|
RU2717596C1 |
POLYESTER-WOOD COMPOSITION WITH FOAMED POLYSTYRENE WASTES | 2011 |
|
RU2465296C1 |
NANOMODIFIED POLYMER COMPOSITE | 2012 |
|
RU2488563C1 |
TUBE AND METHOD OF ITS PRODUCTION | 2011 |
|
RU2483924C2 |
POLYMER POWDER COMPOSITION FOR SUPERHYDROPHOBIC COATING AND METHOD OF OBTAINING SUPERHYDROPHOBIC COATING | 2013 |
|
RU2547754C2 |
HYDROINSULATING COMPOSITION | 1988 |
|
SU1624989A1 |
COMPOSITION FOR MOULDING STRUCTURAL AND FINISHING MATERIALS WITH ANTI-ICING PROPERTIES | 2011 |
|
RU2466170C1 |
PROTECTIVE EPOXIDE-WOOD COAT FOR FOAM POLYSTYRENE | 2007 |
|
RU2368633C2 |
METHOD OF DECORATIVE ARTICLES PRODUCTION | 2002 |
|
RU2219064C1 |
Authors
Dates
2016-02-10—Published
2014-09-08—Filed