FIELD: ceramic industry.
SUBSTANCE: invention relates to compositions of ceramic mixtures used in making facade tiles. Ceramic mixture contains, wt%: brick clay 83.0-84.0; blast-furnace slag 10.0-13.0; talc 4.0-6.0. Blast-furnace slag is characterised by following chemical composition, wt%: SiO2 36.0-41.0; Al2O3 8.0-11.0; FeO 0.2-0.7; CaO 40.0-48.0; MgO 6.0-10.0; MnO 0.1-1.0; SO3 0.5-2.2. Annealing temperature of articles is 950-970 °C.
EFFECT: technical result is low annealing temperature of articles.
1 cl, 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| CERAMIC MIXTURE | 2015 |
|
RU2582141C1 |
| CERAMIC MASS FOR MAKING OF FLOOR TILES | 2008 |
|
RU2372310C1 |
| CERAMIC MIXTURE FOR MAKING TILES | 2010 |
|
RU2415104C1 |
| CERAMIC MASS | 2013 |
|
RU2515645C1 |
| CERAMIC MASS FOR TILE MANUFACTURING | 2012 |
|
RU2499781C1 |
| CERAMIC MASS | 2013 |
|
RU2517401C1 |
| GLASE | 2010 |
|
RU2418771C1 |
| CERAMIC MASS | 2009 |
|
RU2407717C1 |
| CERAMIC MIXTURE FOR MAKING FACING TILES | 2009 |
|
RU2405754C1 |
| RAW MIXTURE FOR MAKING AGGLOPORITE | 2009 |
|
RU2393126C1 |
Authors
Dates
2016-04-20—Published
2015-04-22—Filed