FIELD: construction.
SUBSTANCE: invention relates to construction materials and articles, namely to a method of preparing asphalt mix. Method of preparing asphalt mix containing bitumen in the amount of 3-9 wt%, hydrolyzed lignin with the fraction from 0 to 2.5 mm with the moisture content of 10-50 % in the amount of 3-10 wt% and a mineral material, which contains crushed stone in the amount of 30-70 wt% and sand from grinding screenings - the rest involves simultaneous feeding hydrolyzed lignin and heated up to 130-150 °C bitumen binder to the mixer with heated up to 130-150 °C mineral material. In another version hydrolytic lignin is fed immediately before injection of the heated bitumen binder to the mixer with the heated mineral material.
EFFECT: technical result is higher strength, shear resistance and crack resistance of the asphalt-concrete mixture, as well as reduced mineral materials heating temperature.
2 cl, 3 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
ASPHALT-CONCRETE MIXTURE | 2016 |
|
RU2611801C1 |
METHOD OF PRODUCING COLD ASPHALT CONCRETE MIXTURE BASED ON MODIFIED POLYMER-BITUMEN COMPOSITION | 2023 |
|
RU2824525C1 |
METHOD FOR PRODUCING POLYMERASPHALT CONCRETE MIXTURE | 2020 |
|
RU2749771C1 |
ASPHALT CONCRETE | 2023 |
|
RU2799927C1 |
ASPHALT CONCRETE MIXTURE | 2001 |
|
RU2192399C2 |
ASPHALT CONCRETE | 2023 |
|
RU2814397C1 |
METHOD OF ASPHALT CONCRETE MIXTURE PREPARATION | 2023 |
|
RU2817010C1 |
ASPHALT CONCRETE MIX | 2021 |
|
RU2777276C1 |
ASPHALT CONCRETE | 2020 |
|
RU2755172C1 |
RUBBERISED VIBRO CAST ASPHALT MIX | 2010 |
|
RU2435743C1 |
Authors
Dates
2016-12-10—Published
2015-05-05—Filed