FIELD: chemistry.
SUBSTANCE: two layers of glaze suspension are applied successively, dried and burned. Before applying the lower layer of opacified glaze suspension, silicon carbide screened through sieve No 008 in amount of 0.5-5% of suspension weight is introduced in it. Initial softening temperature of the top layer of transparent glaze suspension is lower than softening temperature of the lower layer by 30-50°C. The lower glaze layer is applied by dipping or coating, the top layer is applied by spraying.
EFFECT: simplified technology for production of articles.
2 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR OBTAINING CRACKLE GLAZE ON SURFACE OF CERAMIC ARTICLE /VERSIONS/ | 2015 |
|
RU2609488C1 |
METHOD TO PRODUCE DECORATIVE GLAZING COATING ON SURFACE OF CERAMIC ITEM | 2011 |
|
RU2487104C1 |
METHOD OF GLASING CERAMIC ARTICLES | 2010 |
|
RU2439038C1 |
METHOD OF DOUBLE LAYER GLAZING OF CERAMIC ITEMS | 2007 |
|
RU2345047C2 |
METHOD OF OBTAINING DECORATIVE GLAZE COATING ON SURFACE OF CERAMIC ARTICLE | 2011 |
|
RU2480436C1 |
METHOD OF GLASING CERAMIC ARTICLES | 2009 |
|
RU2415826C1 |
BESFRITE GLAZE | 2006 |
|
RU2334729C1 |
GLASE COMPOSITION | 2009 |
|
RU2418772C1 |
METHOD OF PRODUCTION OF CERAMIC ART OBJECT | 2007 |
|
RU2333107C1 |
PRODUCTION METHOD OF CRACKLE GLAZE ON SURFACE OF CERAMIC PRODUCT | 2008 |
|
RU2363670C1 |
Authors
Dates
2017-02-02—Published
2015-12-07—Filed