FIELD: construction.
SUBSTANCE: concrete mix, comprising Portland cement, crushed stone, microfiller in the form of limestone, superplasticizer and water. The crushed stone is rubble of limestone with the fraction 5-20 mm, the microfiller is a limestone screening of the fraction below 0.16 mm, the fine filler from limestone screenings of the fractions 5.0-0.63 mm and 0.63-0.16 mm, the superplasticizer C3 based on the product of condensation naphthalene sulphonic acid with formaldehyde, at the following content, wt %: Portland cement 12.1-14.1, 10.5 mm crushed limestone fractions 35-40 , fine filler from limestone screenings of the fraction 5 - 0.63 mm 18.15-20.15 fine filler from limestone screenings of the fraction 0.63-0.16 mm 14.52-15.89, microfill from limestone screenings of the fraction below 0.16 mm 7-8.87, C3 superplasticizer 0.06-0.141 water - the rest.
EFFECT: improved homogeneity of the concrete mix by reducing the peelability.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
CONCRETE MIX | 2021 |
|
RU2771650C1 |
SELF-COMPACTING CONCRETE MIXTURE | 2016 |
|
RU2632795C1 |
SELF-CONSISTENT CONCRETE PRODUCTION METHOD AND CONCRETE MIXTURE | 2017 |
|
RU2659290C1 |
CONCRETE MIX | 2021 |
|
RU2782653C1 |
CONCRETE MIXTURE | 2009 |
|
RU2435746C2 |
CONCRETE MIXTURE | 2013 |
|
RU2525565C1 |
CONCRETE MIXTURE | 2009 |
|
RU2439020C2 |
DRY CONSTRUCTION MIX | 2022 |
|
RU2786931C1 |
SELF-COMPACTING CONCRETE MIXTURE AND METHOD FOR ITS PREPARATION | 2021 |
|
RU2775294C1 |
CONCRETE MIXTURE | 2011 |
|
RU2461524C1 |
Authors
Dates
2017-03-01—Published
2015-11-16—Filed