FIELD: construction.
SUBSTANCE: method for manufacturing wood concrete consists in pre-treatment of wood aggregate in the 4% solution of sodium hydroxide at the temperature of 50-60°C and simultaneous ultrasonic treatment with the frequency of 30-40 kHz for 20-30 minutes; then, after the NaOH solution is drained, the wood aggregate is flushed with water.
EFFECT: increasing physical and mechanical characteristics of products.
1 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING WOOD CONCRETE | 2019 |
|
RU2746720C2 |
WOOD-CONCRETE MIXTURE | 2015 |
|
RU2602279C1 |
CRUDE MIXTURE FOR MANUFACTURING WOOD CONCRETE | 2015 |
|
RU2593608C1 |
RAW MIX FOR PREPARING ARBOLITE AND METHOD OF MANUFACTURE THEREOF | 1998 |
|
RU2153478C1 |
BUILDING MATERIAL BASED ON PORTLAND CEMENT, TRIPOLI POWDER AND LOGGING WASTES, SAWING AND WOODWORKING | 2019 |
|
RU2716632C1 |
CRUDE MIXTURE FOR MAKING WOOD CONCRETE | 2015 |
|
RU2593836C1 |
RAW MIXTURE FOR PRODUCING ARBOLITE | 0 |
|
SU697485A1 |
RAW MIXTURE FOR MAKING ARBOREOUS CONCRETE | 0 |
|
SU637400A1 |
METHOD FOR MANUFACTURE OF PRODUCTS FROM COMPOSITE MATERIALS, MOSTLY CEMENT WOOD | 2007 |
|
RU2345886C2 |
RAW MATERIAL MIXTURE FOR PRODUCTION OF HEAT INSULATING LIGHT CONCRETE | 2008 |
|
RU2377210C2 |
Authors
Dates
2017-05-29—Published
2016-05-11—Filed