FIELD: chemistry.
SUBSTANCE: method for control of rheology of cement compositions with delayed setting comprises preparation of a cement composition with delayed setting. For this purpose, water, pumice stone, slaked lime and retarder are used. Shear stress is applied to the cement composition with delayed setting in an amount sufficient to prevent radical solids precipitation. Storage of cement with delayed setting as of a pumped liquid is provided for at least 1 day. The cement composition with delayed setting is activated. The cement composition with delayed setting is injected into the subterranean formation the ability for the cement compositions with delayed setting to harden in the subterranean formation is provided.
EFFECT: increased efficiency of manufacture and application of cement compositions with delayed setting.
20 cl, 3 dwg, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
ACTIVATORS FOR HARDENING CEMENT FOR CEMENT COMPOSITIONS WITH DISABLED HARDENING AND RELATED METHODS | 2014 |
|
RU2637347C2 |
TWO-COMPONENT CEMENT COMPOSITIONS WITH DELAYED SETTING | 2014 |
|
RU2632086C1 |
CEMENT SETTING ACTIVATORS FOR CEMENT COMPOSITIONS AND CORRESPONDING METHODS | 2014 |
|
RU2635413C2 |
SET-DELAYED PUMICE-CONTAINING CEMENT COMPOSITIONS AND CORRESPONDING METHODS | 2014 |
|
RU2638678C2 |
SLOWLY SOLIDIFYING CEMENT COMPOSITIONS CONTAINING PUMICE AND RELATED METHODS | 2013 |
|
RU2586517C2 |
FOAMING OF SET-DELAYED CEMENT COMPOSITIONS COMPRISING PUMICE AND HYDRATED LIME | 2014 |
|
RU2655669C2 |
CEMENT SETTING ACTIVATOR FOR CEMENT COMPOSITIONS WITH RETARDED SETTING AND RELATED METHODS | 2014 |
|
RU2618540C1 |
DECREASING IMPURITY OF CEMENT COMPOSITIONS WITH SLOW SHINDING CONTAINING PEMOUS AND SULFUR LIME | 2014 |
|
RU2634129C2 |
PLACING A FLUID COMPRISING KILN DUST IN A WELLBORE THROUGH A BOTTOM HOLE ASSEMBLY | 2014 |
|
RU2657276C1 |
METHOD TO USE COMPOSITIONS INCLUDING CEMENT KILN DUST AND CAPABLE OF SETTING | 2006 |
|
RU2460870C2 |
Authors
Dates
2017-06-07—Published
2013-09-09—Filed