FIELD: construction.
SUBSTANCE: charge for obtaining foamed glass contains the following components, wt %: sheet glass battle 94.0-97.0; powder of sewage sludge 1.5-3.5; lithium-cobalt-oxide compound 1.0-3.0. 2 pr.
EFFECT: expansion of raw materials base, decrease in foaming temperature.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
CHARGE FOR OBTAINING FOAM GLASS | 2016 |
|
RU2627788C1 |
COMPOSITION OF FOAMED GLASS COMPOSITE | 2015 |
|
RU2592002C1 |
METHOD OF PRODUCTION OF FOAM GLASS | 2013 |
|
RU2522606C1 |
CRUDE MIXTURE FOR PRODUCING BLOCK FOAMED GLASS | 2024 |
|
RU2824109C1 |
CHARGE FOR PRODUCING FOAMED GLASS | 2017 |
|
RU2684654C2 |
METHOD FOR MANUFACTURING OF GLASED GLASS FOAM | 2010 |
|
RU2431619C1 |
BLEND FOR PREPARING FOAM GLASS | 1998 |
|
RU2149146C1 |
CHARGE FOR PRODUCTION OF GLASS FOAM | 2007 |
|
RU2357933C2 |
METHOD OF PRODUCTION OF FOAMED GLASS | 2005 |
|
RU2291845C2 |
TWO-LAYER BUILDING MATERIAL MANUFACTURE TECHNIQUE | 0 |
|
SU1740336A1 |
Authors
Dates
2017-08-11—Published
2016-05-26—Filed